Old 1/15/12, 9:16 PM
Robert A. Jack Robert A. Jack is offline
InterNACHI Member
 
Join Date: Oct 2006
Location: Guilford, VT
Posts: 63
Default galvanic corrosion?

Can anyone explain if this corrosion is a problem. I’m assuming it is a galvanic type corrosion. If not cleaned, can this result in a leak?
Attached Thumbnails
galvanic-corrosion-p1290144.jpg  
Reply With Quote
Need a home inspection in Wisconsin? Check out InterNACHI's listing of Wisconsin certified home inspectors. Or, find a home inspector anywhere in the world with our inspection search engine.
  #2  
Old 1/15/12, 9:25 PM
Roy D. Cooke, Sr's Avatar
Roy D. Cooke, Sr Roy D. Cooke, Sr is offline
InterNACHI Member
 
Join Date: Aug 2003
Location: Brighton, ON
Posts: 14,621
Default Re: galvanic corrosion?

Yes it will .


I would look for an electrical low voltage electrical leak .... Roy...
Possible DC
Reply With Quote
  #3  
Old 1/15/12, 9:45 PM
Robert A. Jack Robert A. Jack is offline
InterNACHI Member
 
Join Date: Oct 2006
Location: Guilford, VT
Posts: 63
Default Re: galvanic corrosion?

Thanks Roy. I will recommend that.
Reply With Quote
  #4  
Old 1/15/12, 9:52 PM
Michael Larson's Avatar
Michael Larson Michael Larson is offline
InterNACHI Member
 
Join Date: May 2006
Location: Hudson, WI including the Twin Cities of MN
Posts: 32,090
Default Re: galvanic corrosion?

Quote:
Originally Posted by rjack1 View Post
Thanks Roy. I will recommend that.
What?

They need plumber not some hack with a meter.



You can argue with intelligent people but to argue with a mush head is like trying to grab fog-Thomas Sowell

Never underestimate the difficulty of changing false beliefs by facts. - Henry Rosovsky-Harvard

Michael Larson
Hudson, WI

Services provided in East MN and West WI

Reply With Quote
  #5  
Old 1/15/12, 10:38 PM
Charley L. Bottger's Avatar
Charley L. Bottger Charley L. Bottger is offline
InterNACHI Member
 
Join Date: Apr 2004
Location: Marland, OK
Posts: 4,187
Default Re: galvanic corrosion?

Looks to me like the packing gland leaked until it scabbed closed seen a million just like it



Freedom Express Inspections LLC
CMOR Thermography Certified Level III #8486
freedomexpressinspections.com
www.oklahomathermalinfraredimaging.com
freedomexpress495@att.net
NACHI Member
Okla. State DEQ Environmental Phase One Certified
Master HVAC Mechanic (Retired)
Certified Universal Freon by 40CFR 82 Sub-part F
State License # 130
Serving the States of Okla, Texas, Kansas, Missouri , Arkansas and New Mexico with Commercial Inspections,Thermal Imaging
Reply With Quote
  #6  
Old 1/15/12, 10:45 PM
Michael Larson's Avatar
Michael Larson Michael Larson is offline
InterNACHI Member
 
Join Date: May 2006
Location: Hudson, WI including the Twin Cities of MN
Posts: 32,090
Default Re: galvanic corrosion?

Charley, I see copper galvy, black and brass in the pic.



You can argue with intelligent people but to argue with a mush head is like trying to grab fog-Thomas Sowell

Never underestimate the difficulty of changing false beliefs by facts. - Henry Rosovsky-Harvard

Michael Larson
Hudson, WI

Services provided in East MN and West WI

Reply With Quote
  #7  
Old 1/15/12, 10:56 PM
Charley L. Bottger's Avatar
Charley L. Bottger Charley L. Bottger is offline
InterNACHI Member
 
Join Date: Apr 2004
Location: Marland, OK
Posts: 4,187
Default Re: galvanic corrosion?

Quote:
Originally Posted by mlarson View Post
Charley, I see copper galvy, black and brass in the pic.
I do see it also but look at the packing gland corrosion goes all the way to the hand wheel



Freedom Express Inspections LLC
CMOR Thermography Certified Level III #8486
freedomexpressinspections.com
www.oklahomathermalinfraredimaging.com
freedomexpress495@att.net
NACHI Member
Okla. State DEQ Environmental Phase One Certified
Master HVAC Mechanic (Retired)
Certified Universal Freon by 40CFR 82 Sub-part F
State License # 130
Serving the States of Okla, Texas, Kansas, Missouri , Arkansas and New Mexico with Commercial Inspections,Thermal Imaging
Reply With Quote
  #8  
Old 1/15/12, 11:05 PM
Michael Larson's Avatar
Michael Larson Michael Larson is offline
InterNACHI Member
 
Join Date: May 2006
Location: Hudson, WI including the Twin Cities of MN
Posts: 32,090
Default Re: galvanic corrosion?

Quote:
Originally Posted by cbottger View Post
I do see it also but look at the packing gland corrosion goes all the way to the hand wheel
Yep, but there is plenty to call out there.



You can argue with intelligent people but to argue with a mush head is like trying to grab fog-Thomas Sowell

Never underestimate the difficulty of changing false beliefs by facts. - Henry Rosovsky-Harvard

Michael Larson
Hudson, WI

Services provided in East MN and West WI

Reply With Quote
  #9  
Old 1/16/12, 3:22 PM
Nick Gromicko's Avatar
Nick Gromicko Nick Gromicko is offline
InterNACHI Member
 
Join Date: Aug 2002
Location: Valley Forge, PA
Posts: 30,614
Default Re: galvanic corrosion?

http://www.nachi.org/galvanic-corrosion.htm



Nick Gromicko, Certified Master Inspector

Find a Home Inspector
"Just as iron sharpens iron, one man sharpens another." Proverbs 27:17
Reply With Quote
  #10  
Old 1/16/12, 3:43 PM
Charley L. Bottger's Avatar
Charley L. Bottger Charley L. Bottger is offline
InterNACHI Member
 
Join Date: Apr 2004
Location: Marland, OK
Posts: 4,187
Default Re: galvanic corrosion?

Quote:
Originally Posted by mlarson View Post
Yep, but there is plenty to call out there.
I don't disagree with that but the green comes from a water leak guess we could talk about the super bowl that seems high on some threads



Freedom Express Inspections LLC
CMOR Thermography Certified Level III #8486
freedomexpressinspections.com
www.oklahomathermalinfraredimaging.com
freedomexpress495@att.net
NACHI Member
Okla. State DEQ Environmental Phase One Certified
Master HVAC Mechanic (Retired)
Certified Universal Freon by 40CFR 82 Sub-part F
State License # 130
Serving the States of Okla, Texas, Kansas, Missouri , Arkansas and New Mexico with Commercial Inspections,Thermal Imaging
Reply With Quote
Reply

Thread Tools

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are On


Similar Threads
Thread Thread Starter Forum Replies Last Post
Galvanic corrosion of a ufer ground kshepard Electrical Inspections 28 11/7/11 3:37 AM
Galvanic Corrosion. New InterNACHI inspection article. gromicko Plumbing Inspections 2 9/16/10 12:21 AM
Galvanic Corrosion dgagneur Inspecting HVAC Systems 4 9/13/10 10:41 PM
New article on galvanic corrosion inxil InterNACHI & RealMatcher Blogs 0 9/13/10 8:40 PM
Soldered pipe supports causing corrosion kshepard Plumbing Inspections 7 12/3/06 2:30 PM


All times are GMT -4. The time now is 1:37 PM.


Popular Sections

:

All Sections

Inspection News

InterNACHI Membership

Inspection Standards

Inspection Education

InterNACHI Inspectors

Inspection Links

 

 

 

NACHI.ORG Statistics

 

 

no new posts